Processing of Beryllium Oxide Fuels
Description:
Preliminary results from experiments on the dissolution of beryllium metal and sintered UO2-BeO fuel pellets are reported. In all cases the pellets were fired in hydrogen at 1650-1800°C. Uranium, from UO2-BeO pellets containing more than 60% UO2, is readily leached with boiling 6-13 M HNO3 in about 6 hr. The BeO in these pellets dissolves only slowly in nitric acid; however, in 8 M HNO3-0.2M NaF, it dissolves at about the same rate as the UO2. Sintered pellets containing less than 10% UO2 do no…