Stress corrosion cracking of candidate waste container materials; Final report Page: 18 of 86
76 p.View a full description of this report.
Extracted Text
The following text was automatically extracted from the image on this page using optical character recognition software:
10
---- ------ 76.20 ---
6.35 DIA.
38.1
..-. .-.-*. __ . . - - 11.11 DIA.
-- 9.53
-19.05
TWO THROUGH
HOLES 0.8 TO 0.9
Fig. 1. FabricatIon Drawing for Base Metal SSRT
Specimen. Dimensions are in mm.
76.20 -
6.35 DIA.
9.53 -I - 38.1 - -
-.._. --- -- .... - . - 11.11 DIA.
- LOCATE EDGE OF THIS
0.8 TO 0.9THROUGH HOLE
APPROX. o.A FROM WELD
0.8 to 0.9
THROUGH HOLE 0.8 to 0.9 THROUGH HOLE
IN CENTER OF WELD
Flg. 2. FabrIcation Drawing for Gas-Metal-Arc Welded
Specimen. Dtinensions are In mm.
Upcoming Pages
Here’s what’s next.
Search Inside
This report can be searched. Note: Results may vary based on the legibility of text within the document.
Tools / Downloads
Get a copy of this page or view the extracted text.
Citing and Sharing
Basic information for referencing this web page. We also provide extended guidance on usage rights, references, copying or embedding.
Reference the current page of this Report.
Park, J. Y.; Maiya, P. S.; Soppet, W. K.; Diercks, D. R.; Shack, W. J. & Kassner, T. F. Stress corrosion cracking of candidate waste container materials; Final report, report, June 1, 1992; Illinois. (https://digital.library.unt.edu/ark:/67531/metadc625520/m1/18/: accessed July 16, 2024), University of North Texas Libraries, UNT Digital Library, https://digital.library.unt.edu; crediting UNT Libraries Government Documents Department.