The Ductility of Brazed Stainless Steel Joints

Description: Abstract: "The ductility of Type 310 stainless steel T-joints brazed with GE-62 brazing alloy was measured at room temperatures 1200, 1650, and 1800 F. The measure of ductility was taken as the plastic axial strain required to crack braze fillets in T-section tensile specimens. At elevated temperatures, the ductility of as-brazed joints approximated that of the stainless steel, but at room temperature the brazed joints had only one-tenth the ductility of the base metal. Annealing for 16 hr at 1… more
Date: July 8, 1953
Creator: Saller, Henry A.; Stacy, J. T. & Eddy, N. S.
Partner: UNT Libraries Government Documents Department
open access

Grain Refinement of the As-Cast Uranium-5 w/o Chromium Alloy by Ternary Additions

Description: Abstract: "Refinement of grain size of the base uranium-chromium eutectic alloy (uranium-5 w/o chromium) by ternary additions is discussed. Thirteen additions to the base alloy were investigated, and three additions were found to exhibit worthwhile grain-refinement tendencies. The three alloys, uranium-5 w/o chromium-0.2 w.o molybdenum, uranium-5 w/o chromium-0.2 w/o germanium, and uranium-5 w/o chromium-0.2 w/o niobium, were heat treated to produce final grain-size structures of between 0.015 … more
Date: July 5, 1955
Creator: Saller, Henry A.; Dickerson, Ronald F.; Murr, William E. & Bauer, Arthur A.
Partner: UNT Libraries Government Documents Department