D0 Silicon Upgrade: Calorimeter Installation Bridge Non-Destructive Test Result
Description:
After the central calorimeter was installed on the center beam a cracked weld was found on the bridge. The weld was a partial penetration between the top rail plate and the T-1 steel nose section. The crack is fully across the width of the rail plate and the rail is depressed in a concave shape. That is, the depression is deeper in the center and feathers out to zero at the end of the rail. Upon close inspection it was obvious that there was no penetration of weld metal into the T-1 material. T…