Final Report - Glass Formulation Development and Testing for DWPF High AI2O3 HLW Sludges, VSL-10R1670-1, Rev. 0, dated 12/20/10

PDF Version Also Available for Download.

Description

The principal objective of the work described in this Final Report is to develop and identify glass frit compositions for a specified DWPF high-aluminum based sludge waste stream that maximizes waste loading while maintaining high production rate for the waste composition provided by ORP/SRS. This was accomplished through a combination of crucible-scale, vertical gradient furnace, and confirmation tests on the DM100 melter system. The DM100-BL unit was selected for these tests. The DM100-BL was used for previous tests on HLW glass compositions that were used to support subsequent tests on the HLW Pilot Melter. It was also used to process ... continued below

Creation Information

Kruger, Albert A.; Pegg, I. L.; Kot, W. K.; Gan, H. & Matlack, K. S. November 13, 2013.

Context

This report is part of the collection entitled: Office of Scientific & Technical Information Technical Reports and was provided by UNT Libraries Government Documents Department to Digital Library, a digital repository hosted by the UNT Libraries. More information about this report can be viewed below.

Who

People and organizations associated with either the creation of this report or its content.

Sponsor

Publisher

  • Hanford Site (Wash.)
    Publisher Info: HNF (Hanford Site (HNF), Richland, WA (United States))
    Place of Publication: Richland, Washington

Provided By

UNT Libraries Government Documents Department

Serving as both a federal and a state depository library, the UNT Libraries Government Documents Department maintains millions of items in a variety of formats. The department is a member of the FDLP Content Partnerships Program and an Affiliated Archive of the National Archives.

Contact Us

What

Descriptive information to help identify this report. Follow the links below to find similar items on the Digital Library.

Description

The principal objective of the work described in this Final Report is to develop and identify glass frit compositions for a specified DWPF high-aluminum based sludge waste stream that maximizes waste loading while maintaining high production rate for the waste composition provided by ORP/SRS. This was accomplished through a combination of crucible-scale, vertical gradient furnace, and confirmation tests on the DM100 melter system. The DM100-BL unit was selected for these tests. The DM100-BL was used for previous tests on HLW glass compositions that were used to support subsequent tests on the HLW Pilot Melter. It was also used to process compositions with waste loadings limited by aluminum, bismuth, and chromium, to investigate the volatility of cesium and technetium during the vitrification of an HLW AZ-102 composition, to process glass formulations at compositional and property extremes, and to investigate crystal settling on a composition that exhibited one percent crystals at 963{degrees}C (i.e., close to the WTP limit). The same melter was selected for the present tests in order to maintain comparisons between the previously collected data. The tests provide information on melter processing characteristics and off-gas data, including formation of secondary phases and partitioning. Specific objectives for the melter tests are as follows: Determine maximum glass production rates without bubbling for a simulated SRS Sludge Batch 19 (SB19). Demonstrate a feed rate equivalent to 1125 kg/m{sup 2}/day glass production using melt pool bubbling. Process a high waste loading glass composition with the simulated SRS SB19 waste and measure the quality of the glass product. Determine the effect of argon as a bubbling gas on waste processing and the glass product including feed processing rate, glass redox, melter emissions, etc.. Determine differences in feed processing and glass characteristics for SRS SB19 waste simulated by the co-precipitated and direct-hydroxide methods. The above tests were proposed based on previous tests for WTP in which there were few differences in the melter processing characteristics, such as processing rate and melter emissions, between precipitated and direct hydroxide simulants, even though there were differences in rheological properties. To the extent this similarity is found also for simulants for SRS HLW, the direct hydroxide methods may offer the potential for faster, simpler, and cheaper simulant production. There was no plan to match the yield stress and particle size of the direct hydroxide simulant to that of the precipitated simulant because that would have increased the preparation cost and complexity and defeated the purpose of the tests. These objectives were addressed by first developing a series of glass frits and then conducting a crucible scale study to determine the waste loading achievable for the waste composition and to select the preferred frit. Waste loadings were increased until the limits of a glass property were exceeded experimentally. Glass properties for evaluation included: viscosity, electrical conductivity, crystallinity (including liquidus temperature and nepheline formation after canister centerline cooling (CCC) heat-treatment), gross glass phase separation, and the 7- day Product Consistency Test (PCT, ASTM-1285) response. Glass property limits were based upon the constraints used for DWPF process control.

Language

Item Type

Identifier

Unique identifying numbers for this report in the Digital Library or other systems.

  • Report No.: ORP-56290 Rev 0
  • Grant Number: DE-AC27-08RV14800
  • DOI: 10.2172/1105970 | External Link
  • Office of Scientific & Technical Information Report Number: 1105970
  • Archival Resource Key: ark:/67531/metadc870884

Collections

This report is part of the following collection of related materials.

Office of Scientific & Technical Information Technical Reports

What responsibilities do I have when using this report?

When

Dates and time periods associated with this report.

Creation Date

  • November 13, 2013

Added to The UNT Digital Library

  • Sept. 16, 2016, 12:32 a.m.

Description Last Updated

  • Nov. 1, 2016, 10:53 a.m.

Usage Statistics

When was this report last used?

Yesterday: 1
Past 30 days: 1
Total Uses: 4

Interact With This Report

Here are some suggestions for what to do next.

Start Reading

PDF Version Also Available for Download.

Citations, Rights, Re-Use

Kruger, Albert A.; Pegg, I. L.; Kot, W. K.; Gan, H. & Matlack, K. S. Final Report - Glass Formulation Development and Testing for DWPF High AI2O3 HLW Sludges, VSL-10R1670-1, Rev. 0, dated 12/20/10, report, November 13, 2013; Richland, Washington. (digital.library.unt.edu/ark:/67531/metadc870884/: accessed September 23, 2017), University of North Texas Libraries, Digital Library, digital.library.unt.edu; crediting UNT Libraries Government Documents Department.