Aspects of the Brittle Fracture Failure of a 30-Inch-Id, 30,000-Psi Isostat With Threaded Closure. Metadata

Metadata describes a digital item, providing (if known) such information as creator, publisher, contents, size, relationship to other resources, and more. Metadata may also contain "preservation" components that help us to maintain the integrity of digital files over time.

Title

  • Main Title Aspects of the Brittle Fracture Failure of a 30-Inch-Id, 30,000-Psi Isostat With Threaded Closure.

Creator

  • Author: Pohto, H. A.
    Creator Type: Personal

Publisher

  • Name: Oak Ridge Y-12 Plant
    Place of Publication: Oak Ridge, Tennessee
    Additional Info: Union Carbide Corp., Oak Ridge, Tenn. Y-12 Plant

Date

  • Creation: 1971-01-01

Language

  • English

Description

  • Physical Description: 39 p.

Subject

  • Keyword: N24000* --Engineering
  • Keyword: Pressure Vessels/Failure Of 30-Inch-Id, Brittle Fracture
  • Keyword: No Keywords Pressure Vessels/Failure Of 30-Inch-Id, Brittle Fracture

Source

  • Other Information: UNCL. Orig. Receipt Date: 31-DEC-71

Collection

  • Name: Office of Scientific & Technical Information Technical Reports
    Code: OSTI

Institution

  • Name: UNT Libraries Government Documents Department
    Code: UNTGD

Resource Type

  • Report

Format

  • Text

Identifier

  • Report No.: Y--1758
  • Grant Number: W-7405-ENG-26
  • DOI: 10.2172/4089612
  • Office of Scientific & Technical Information Report Number: 4089612
  • Archival Resource Key: ark:/67531/metadc869847

Note

  • Display Note: Dep. NTIS.