Progress in the Savannah River /sup 238/Pu Fuel Form Program is summarized. Work during this period concentrated on the extensive cracking of the /sup 238/PuO/sub 2/ fuel form prior to encapsulation in the iridium containment shell for heat sources. This cracking results in increased recycle cost and decreased production efficiency. To better understand this cracking, Savannah River Laboratory (SRL) has made an extensive review of the development of /sup 238/PuO/sub 2/ fuel forms from small-scale Multi-hundred Watt (MHW) pellets through the current GPHS full-scale pellet production. Historically, /sup 238/PuO/sub 2/ fuel has almost always been uncracked after hot pressing in …
continued below
Publisher Info:
Du Pont de Nemours (E.I.) and Co., Aiken, SC (USA). Savannah River Lab.
Place of Publication:
Aiken, South Carolina
Provided By
UNT Libraries Government Documents Department
Serving as both a federal and a state depository library, the UNT Libraries Government Documents Department maintains millions of items in a variety of formats. The department is a member of the FDLP Content Partnerships Program and an Affiliated Archive of the National Archives.
Descriptive information to help identify this report.
Follow the links below to find similar items on the Digital Library.
Description
Progress in the Savannah River /sup 238/Pu Fuel Form Program is summarized. Work during this period concentrated on the extensive cracking of the /sup 238/PuO/sub 2/ fuel form prior to encapsulation in the iridium containment shell for heat sources. This cracking results in increased recycle cost and decreased production efficiency. To better understand this cracking, Savannah River Laboratory (SRL) has made an extensive review of the development of /sup 238/PuO/sub 2/ fuel forms from small-scale Multi-hundred Watt (MHW) pellets through the current GPHS full-scale pellet production. Historically, /sup 238/PuO/sub 2/ fuel has almost always been uncracked after hot pressing in a graphite die, but has emerged cracked and fragile from the final heat-treatment furnace. The cracking tendency depends on the microstructure of the fuel form and on the hot pressing conditions used to fabricate it. In general, a microstructure of large intershard porosity is more desirable because it allows internal gas to escape more readily and it can absorb more reoxidation strain. Studies of the GPHS microstructure showed that the internal structures of typical GPHS Pellets fabricated at LANL and in the PEF differed significantly. The LANL pellets had severe density gradients and were extensively cracked.
This report is part of the following collection of related materials.
Office of Scientific & Technical Information Technical Reports
Reports, articles and other documents harvested from the Office of Scientific and Technical Information.
Office of Scientific and Technical Information (OSTI) is the Department of Energy (DOE) office that collects, preserves, and disseminates DOE-sponsored research and development (R&D) results that are the outcomes of R&D projects or other funded activities at DOE labs and facilities nationwide and grantees at universities and other institutions.